Body Paint

Pre-processing of Painting

6-5  

  1. Featheredging

NOTE

  • The paint film damaged area should be sanded flat and smooth.
  • If this is not done correctly the end results will not be acceptable.

Damage to metal surface:

  • Sand the damaged area flat and smooth.
Use the disc sander and #60~#80 disc paper.

  1. Top coat
  2. Intermediate coat
  3. Undercoat
  4. Metal surface
Use the double action sander and #60~#80 disc paper.

  • Sand the area larger than the damaged area.
Use the double action sander and #180~#240 disc paper.

  • If double action sander is not available, use a rubber pad and wet or dry sandpaper.
Use the flexible block and #280, #340, #400, #600 sandpaper.

Damage to undercoat, intermediate coat and top coat:

Sand the damage area flat and smooth

Use the double action sander and #180~#240~#320 disc paper.

  1. Preparation of metal surface

Remove all corrosion from the damaged area.

Use a product that removes corrosion.

  1. Air blowing/degreasing
Use alcohol, wax and grease remover.